Abstract
In response to the cement industry’s ongoing efforts to reduce carbon emissions, Type IL cement has emerged as a sustainable alternative to traditional Type I/II cement. However, limited research has examined the influence of Type IL cementitious systems on the bond strength between seven-wire prestressing strands and surrounding grout or mortar—an essential factor in the performance of prestressed concrete. This study investigates the bond behavior and transfer length of prestressing strands embedded in grout, mortar, and concrete made with five different cementitious systems: Type I/II cement, Type IL cement (containing 8% limestone inter-ground with Type I/II clinker), and intermixed Type IL where Type I/II cement was mixed with appropriate amounts of separately ground limestone powder to reach the desired limestone content (by % weight). Pullout tests were conducted to evaluate bond strength at 0.01-inch and 0.10-inch strand slips, representing initial and residual bond performance. The results showed that, in grout specimens, the intermixed Type IL mixtures with 8% and 15% limestone content outperformed both Type I/II and Type IL, while the intermixed Type IL (with 20% limestone content) mixture showed reduced bond strength. In contrast, all three intermixed Type IL mixtures - with 8%, 15%, and 20% limestone content - demonstrated higher bond strength in mortar compared to both Type I/II and Type IL mixtures. Type IL cement exhibited slightly higher early-age bond strength than Type I/II at a 0.01-inch slip, but lower bond resistance at a 0.10-inch slip. In addition to pullout testing, the transfer length of pretensioned concrete beams was estimated using Whittemore gauge measurements. The results indicated that concrete produced using Type I/II and intermixed Type IL with 8% limestone content cements developed shorter transfer lengths than Type IL cement at both tension release and 28 days, indicating improved bond performance and more efficient force transfer. All concrete mixtures met the required compressive strength and workability benchmarks, demonstrating the potential of limestone-modified systems as viable, sustainable alternatives for prestressed concrete applications.